Efecto de la concentración de tres engrasantes en las propiedades físicas del cuero vacuno curtido al cromo

dc.contributor.advisorAscón Dionicio, Gregorio Mayer
dc.contributor.authorVillena Mozo, Marco Antonio
dc.date.accessioned4/26/2017 10:32
dc.date.available4/26/2017 10:32
dc.date.issued2013
dc.descriptionThe purpose of this research is to know the best application conditions of three types of oiling, by applying experimental design model, simplex centroid design expanded, so that it can provide in the leather the best properties. We performed a comparative study between Synthetic oil, taken as reference lubrication, and three types of lubricants polymer of acrylic esters, sulfated semisynthetic fat and lecithin. The results show that the greater degree of softness (higher than 4.1 mm) is obtained by applying 0 to 1.7% of acrylic ester polymer, from 0 to 1.7% sulphited semisynthetic fat, from 6.7 to 10% lecithin; The greatest variation of thick (higher than 1.3 mm) is obtained by applying 6 to 10% of acrylic ester polymer, from 0 to 2.5% sulphited semisynthetic fat, 0 to 1.5% lecithin; the higher tensile strength (higher than 240 N) is obtained applying 0 to 1% of acrylic ester polymer, from 0 to 2% sulphited semisynthetic fat, 7 to 10% lecithin; The tear resistance (greater than 120 N) is obtained by applying 0 to 1% of acrylic ester polymer , from 0 to 1% sulphited semisynthetic fat, 8 to 10% lecithin.es_PE
dc.description.abstractEl propósito del presente trabajo de investigación, es conocer las mejores condiciones aplicativas de tres tipos de engrasantes, mediante la aplicación de un diseño de modelo experimental, diseño simplex centroide ampliado, de manera que se puedan proporcionar en los cueros las mejores propiedades. Se realizó un estudio comparativo entre un aceite sintético, como engrase de referencia y tres tipos de engrasantes polímero de esteres acrílicos, grasa semisintética sulfitada y lecitina. Los resultados obtenidos muestran que el mayor grado de blandura (mayor a 4.1 mm) se obtiene aplicando de 0 a 1.7% de polímero de esteres acrílicos, de 0 a 1.7% grasa semisintética sulfitada, de 6.7 a 10% lecitina; la mayor variación de espesor (mayor a 1.3 mm) se obtiene aplicando 6 a 10 % de polímero de esteres acrílicos, de 0 a 2.5% grasa semisintética sulfitada, de 0 a 1.5% lecitina; la mayor resistencia a la tracción (mayor a 240 N) se obtiene aplicando 0 a 1% de polímero de esteres acrílicos, de 0 a 2% grasa semisintética sulfitada, de 7 a 10% lecitina; la mayor resistencia al desgarro (mayor a 120 N) se obtiene aplicando 0 a 1% de polímero de esteres acrílicos, de 0 a 1% grasa semisintética sulfitada, de 8 a 10% lecitinaes_PE
dc.description.uriTesises_PE
dc.identifier.urihttps://hdl.handle.net/20.500.14414/7515
dc.language.isospaes_PE
dc.publisherUniversidad Nacional de Trujilloes_PE
dc.relation.ispartofseriesTAGI;329
dc.rightsinfo:eu-repo/semantics/openAccesses_PE
dc.rights.urihttp://creativecommons.org/licenses/by-nc-nd/2.5/pe/es_PE
dc.sourceUniversidad Nacional de Trujilloes_PE
dc.sourceRepositorio institucional - UNITRUes_PE
dc.subjectCuero vacunoes_PE
dc.subjectCurtidoes_PE
dc.subjectCromoes_PE
dc.titleEfecto de la concentración de tres engrasantes en las propiedades físicas del cuero vacuno curtido al cromoes_PE
dc.typeinfo:eu-repo/semantics/bachelorThesises_PE
thesis.degree.disciplineZootecniaes_PE
thesis.degree.grantorUniversidad Nacional de Trujillo. Facultad de Ciencias Agropecuariases_PE
thesis.degree.levelTítulo Profesionales_PE
thesis.degree.nameIngeniero Zootecnistaes_PE
Files
Original bundle
Now showing 1 - 1 of 1
No Thumbnail Available
Name:
Villena Mozo Marco Antonio.pdf
Size:
4.02 MB
Format:
Adobe Portable Document Format
Description:
License bundle
Now showing 1 - 1 of 1
No Thumbnail Available
Name:
license.txt
Size:
1.71 KB
Format:
Item-specific license agreed upon to submission
Description: